Corrosivity to Metals:
Sodium hypochlorite solutions (15%) are corrosive to brass (aluminum, naval and silicon) bronze,
carbon steel, cast iron, Hastelloy, Inconel, nickel, stainless steels (types 304/347, 316 and 400
series) and silicon copper. Concentrated sodium hypochlorite is corrosive to most metals,
including aluminum, copper, brass, bronze, carbon steel, Hastelloy, Inconel, lead, Monel, nickel
and stainless steel type 400 series. Sodium hypochlorite solutions are not corrosive to tantalum,
titanium and zirconium. Dilute solutions are not corrosive to Hastelloy C/C-276 (10%), Incolloy
(5%) and high silicon iron.
Corrosivity to Non-Metals:
Sodium hypochlorite solutions attack some plastics (such as nylon, Bisphenol A-fumarate and
isophthalic polyesters), elastomers (such as soft rubber, neoprene and nitrile Buna-N) and
coatings (such as coal tar epoxy, epoxy and vinyls).
Sodium hypochlorite solutions do not attack acrylonitrile-butadiene-styrene (ABS), Butyl rubber,
isoprene, hard rubber, natural rubber, polyvinyl chloride (PVC), chlorinated polyvinyl chloride
(CPVC), polyethylene, polypropylene, polystyrene, Teflon and Viton.
Don't worry about galv steel, done many chequerplate staircases caked in algae and sprayed with a hypo mix, doesn't need to sit longer than 10 mins. It'll be fine.